Description: Sintered compacts without further heat treatment were fabricated at 540 °C, 570 °C, 600 °C and 650 °C (below the melting temperature of aluminium) via spark plasma sintering (SPS). Ti and Al in a prop ... More
Full Text: Full Text
Date: 2016
Language: en
Type: Text
Identifier: tut:4811
Description: The possibility of using the low pressure cold spray system to deposit SiC-based cermet on Ti-6Al-4V was investigated at 0.99 Mpa for 450, 500 and 550 °C. The characterizations of the coatings reveal ... More